All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium Carbonate 3.89
Dolomite 5.56
Gerstley Borate 11.12
Whiting 8.34
Wood Ash (soft wood) 1.00
Zinc Oxide 1.67
Kona F-4 Feldspar 41.72
EPK Kaolin 1.67
Silica 25.03
Add Amount
Tin Oxide 0.83
Copper Oxide 0.42

Instructions

Originally published in the October 2010 issue of Ceramics Monthly.