All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 24.00
Silica 34.00
Kaolin 14.00
Gerstley Borate 2.00
Zinc Oxide 2.00
Custer Feldspar 24.00
Add Amount
Tin Oxide 2.00
Copper Carbonate 2.00
Cobalt Carbonate 0.50

Instructions


Nice even purple