All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 15.46
Monzonite 64.56
Kentucky Ball Clay (OM 4) 3.32
Silica 16.66

Instructions

Published in "Larry Davidson" by Lyn Kidder, in the Jan 2000 issue of Ceramics Monthly.