All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Spodumene 11.11
Grolleg Kaolin 44.44
New Foundry Hill Créme 44.45
Add Amount
Zircopax 11.11

Instructions

Published in "Soda Firing Slip & Glaze" in the Dec 2014 issue of Ceramics Monthly.

Image shown is porcelain, slip, Ted's New Orange Slip, soda fired to cone 10.
Best when sprayed thinly across the surface of bisque-fired work.