All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 20.00
Grolleg Kaolin 20.00
Helmer Kaolin 20.00
OM 4 Ball Clay 20.00
Tile 6 Kaolin 20.00

Instructions


Apply thin layer over buff stoneware by spraying. Results range from orange to gray to brown.

This recipe was shared by Stuart Gair in the April 2021 issue of Ceramics Monthly.