All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Laguna WC-617, #16 50.00
White Distilled Vinegar 50.00

Instructions

Joining slip for attachments.

Published in "In the Service of Food" by Adrienne Eliades, in the J/F 2017 issue of Pottery Making Illustrated.