All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 5.00
Ferro Frit 3124 20.00
Ball Clay 25.00
EPK Kaolin 12.50
Georgia Kaolin 12.50
Pyrophyllite 5.00
Silica 20.00
Add Amount
Zircopax 5.00

Instructions

Published in "Clay & Glaze: Low to High" by Bede Clarke, in the Sep 2014 issue of Ceramics Monthly.