All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting (Kulu) 25.00
Potash Feldspar 25.00
Kaolin (G1) 25.00
Silica 25.00
Add Amount
Copper Oxide 0.50
Red Iron Oxide 3.00

Instructions

Shared by Martin Swart in "Working Potter Glazes" in the June 2016 issue of Ceramics Monthly, page 68.
Test using whiting, potassium feldspar (like Custer feldspar), and kaolin (like EPK kaolin) available from a local supplier. To make a gray/blue glaze, substitute cobalt oxide at 0.5% for the copper oxide.