All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Albany Slip 75.00
Nepheline Syenite 25.00
Add Amount
Cobalt Carbonate 5.00

Instructions

This is a glaze from Tom Coleman.

The test tile is Coleman Porcelain fired in reduction.
Alberta Slip was used as a substitute for Albany Slip.