All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 15.70
Whiting 11.30
Talc 6.10
Nepheline Syenite 26.20
EPK Kaolin 17.40
Silica 23.30
Add Amount
Erbium Oxide 8.00

Instructions

A high EPK kaolin base that does not show crazing on porcelain.

Originally published in the November 2017 issue of Ceramics Monthly.