All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wollastonite 25.10
Ferro Frit 3124 33.30
EPK Kaolin 34.70
Silica 6.90

Instructions

Published in "Cone 6 Glazes" by Emily Schroeder Willis, in the Oct 2014 issue of Ceramics Monthly.
Include a 6-10 minute hold at the end of the firing. Add 1 to 3% colorant for pastels.