All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Soda Ash 3.30
Kona F-4 Feldspar* 9.00
Nepheline Syenite 37.50
Spodumene 12.70
EPK Kaolin 25.00
OM 4 Ball Clay 12.50

Instructions

Originally published in the November/December 2017 issue of Pottery Making Illustrated.

 
*Substitute Minspar 200 feldspar for the Kona F-4 feldspar, which is no longer available.