All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 18.00
Nepheline Syenite 49.00
EPK Kaolin 8.00
Silica 25.00
Add Amount
Mason Stain 6600 10.00
Tin Oxide 4.00
Zinc Oxide 8.00

Instructions

Originally published in the May 2018 issue of Ceramics Monthly.