All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
EPK Kaolin 50.00
Alumina Hydrate 50.00

Instructions


This recipe can be used at all temperatures.

Mix to clay-like consistency and use in between shelves and stilts.

This recipe was shared by Stuart Gair in the April 2021 issue of Ceramics Monthly.