All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 5.00
Whiting 16.00
Zinc Oxide 5.00
Kona F4 Feldspar (sub Minspar 200 Feldspar) 30.00
EPK Kaolin 14.00
Silica 30.00

Instructions

Image shown is porcelain, Bauer Orange Flashing Slip, commercial underglaze, Shaner Clear Liner Glaze, Oribe Green, soda fired to cone 10-11.

Published in "Soda Surfaces" by Nolan Baumgartner, in the Dec 2014 issue of Ceramics Monthly.