All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Alka-Seltzer Gold (14 tablets) 41.97
Talcum Powder 9.67
Pumice 48.36

Instructions

Published in "Over-the-Counter Glazes" by John Britt, in the Jun 2001 issue of Ceramics Monthly.