All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 20.80
Custer Feldspar 57.10
EPK Kaolin 15.40
Silica 6.70
Add Amount
Titanium Dioxide 10.90
Zinc Oxide 9.90
Bentonite 3.30

Instructions

Published in "Casting Slip & Glazes," in the May 2016 issue of Ceramics Monthly, page 88.

Satin Cream glaze that holds colorants well. Shown here with on the exterior with different stains.
This glaze holds colorants well. For additional colors, try testing commercial stains at 2–8%.