All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Calcium Carbonate 3.00
Dolomite 17.27
Custer Feldspar 32.73
EPK Kaolin 18.36
Silica 28.64
Add Amount
Cobalt Carbonate 0.27
Rutile 8.73

Instructions

Published in "Rutile" by Ryan Coppage, in the October 2017 issue of Ceramics Monthly.
This glaze is great when with a tenmoku glaze over it, but not vice versa.