All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 15.05
Gerstley Borate 9.68
Custer Feldspar 43.01
EPK Kaolin 8.60
Silica 23.66
Add Amount
Zinc 7.53

Instructions

This recipe was shared by Susan Beiner in the December 2018 issue of Ceramics Monthly.
Application can be thin to medium thick. This is a transparent base glaze that works well with stains and oxides.

I use several heavily fluxed base glazes combined with a variety o Mason stains, rare earth oxides, and encapsulated pigments to create palettes of color to glaze in a more painterly manner. Multiple glazes overlap, which influences how the glazes move across the forms. I am continually testing glazes and looking for interesting overlaps. Glaze application is done with a spray gun and bulb syringe. I draw glaze using a bulb syringe to further increase the mixing and melting of the glazes.