All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3124 80.00
EPK Kaolin 10.00
Silica 10.00
Add Amount
Mason Stain 10.00
Bentonite 1.00

Instructions


I used Mason stain #6025 Coral Red as the colorant in the process images.

This recipe was shared by Alan Johnson in the January/February 2021 issue of Pottery Making Illustrated.