All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Borax 5.28
Custer Feldspar 21.05
Ball Clay 15.79
Calcined Kaolin 21.05
EPK Kaolin 15.78
Silica 21.05
Add Amount
Zircopax 5.28

Instructions

Published in "Clay & Glaze: Low to High" by Bede Clarke, in the Sep 2014 issue of Ceramics Monthly.
Apply to bisqueware. To make a black slip, add 2 tablespoons of #6666 Cobalt-free Black Mason stain to one cup of Rhodes Crackle Slip.

Image shows Rhodes Crackle Slip layered under Malcolm Davis Red Shino.