All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Lithium Carbonate 40.00
Ferro Frit 3124 30.00
Zircopax Plus 20.00
Silica 10.00
Add Amount
Copper Carbonate 2.50
Bentonite 1.00

Instructions


Apply by spraying, then remove excess glaze with a dry sponge to reveal the layers beneath.

This recipe was shared by Alan Johnson in the January/February 2021 issue of Pottery Making Illustrated.