All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Kona F-4 Feldspar 34.00
Grolleg Kaolin 40.00
Silica 26.00
Add Amount
Water 35.00
Darvan 0.35

Instructions


Water and Darvan amounts are only approximate will vary. This casting slip was adapted from John Reeve's throwing body. Reeve passes away in 2012. Substitute Minspar 200 feldspar for Kona F-4 feldspar, which is no longer available.