All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Cedar Heights Goldart 30.00
Cedar Heights Redart 50.00
Tennessee Ball Clay #5 20.00
Add Amount
Grog 1.50

Instructions

Published in "The Pottery Shop at Greenfield Village" by Sarah Bailey, in the May 2003 issue of Ceramics Monthly.