All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Laterite Red Clay 100.00

Instructions

Published in "Reduction Cool Slip," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Stephen Heywood.