All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 5.00
Ferro Frit 3110 15.00
Cedar Heights Redart 40.00
Cedar Heights Goldart 20.00
Tennessee #1 SPG 5.00
Silica 15.00
Add Amount
Barium Carbonate 0.20
Daravan #7 0.50

Instructions

A red earthenware, highly vitrified, fritware casting slip. Compatible with White Decorating Slip and Clear Glaze.

Published in "Cone 04 Glazes" by Anna and Kevin Ramsay, in the Feb 2017 issue of Ceramics Monthly.
Ferro frit 3110 is a high-alkali, low-boron, and low-alumina frit manufactured in the US.