All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 20.00
Ferro Frit 3134 14.00
Nepheline Syenite 18.00
Kentucky Ball Clay 18.00
Silica 30.00
Add Amount
Tin Oxide 7.50
Chrome Oxide 0.20
Cobalt Carbonate 0.25

Instructions

Published in "Chrome Oxide" by John Britt, in the Nov 2012 issue of Ceramics Monthly.  


From Mastering Cone 6 Glazes by John Hesselberth and Ron Roy