All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 10.71
Wollastonite 7.14
Foundry Hill Creme 7.14
Hawthorn Bond (20 Mesh) 10.71
Cedar Heights Redart Clay 35.74
Lizella Clay 21.42
OM 4 Ball Clay 7.14
Add Amount
Fine Grog 7.14
Medium Grog 3.57

Instructions


Using terra-cotta clays for tile presents problems such as high porosity, and poor freeze/thaw properties. While it is not a particularly durable clay, traditionally terra-cotta bodies have defined much of the global tile aesthetic and are ubiquitous with the architecture of many cultures.

This recipe was shared by Forrest Lesch-Middelton in the October 2020 issue of Ceramics Monthly.