All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 5.56
Ferro Frit 3124 22.22
Grolleg Kaolin 33.33
OM 4 Ball Clay 27.78
Silica 11.11
Add Amount
Zircopax 5.56

Instructions

This recipe was developed by Wally Bivins for Pottery Northwest.