All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 6.90
Ferro Frit 3124 6.90
Cedar Heights Redart 34.50
Newman Red Fireclay 17.20
OM 4 Ball Clay 17.30
Carbondale Red 17.20
Add Amount
70-Mesh Sand or Grog 6.90
Multi-Coarse 20-mesh Grog 8.30

Instructions

This Clay Body recipe was developed by Wally Bivins for Pottery Northwest.

Published in "Emerging Artist Recipes" in the May 2017 issue of Ceramics Monthly.