All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wollastonite 2.88
Nepheline Syenite 31.73
EPK Kaolin 23.08
OM 4 Ball Clay 13.46
Silica 28.85
Add Amount
Bentonite 2.88

Instructions