All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 15.60
Magnesium Carbonate 5.70
Minspar 200 Feldspar 51.00
EPK Kaolin 17.10
Silica 10.60
Add Amount
Zircopax 1.00

Instructions

Shared by Brenda Lichman in "Soda Firing Slip & Glaze" in the Dec 2014 issue of Ceramics Monthly.

Image shown is porcelain, slip, Phil's 103 white, soda fired to cone 10.