All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 50.00
Kona F-4 Feldspar 15.00
Spodumene 15.00
Ball Clay (OM 4) 10.00
EPK 10.00
Add Amount
Soda Ash 7.00

Instructions

Found in 2005 Shino Review

Single-dipped renders a light red choral color.

Double-dipped renders a light pastel lavender color
Mixed by hand with equal weight in water as ingredients, then dipped (single and double pictured)