All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 40.00
Nepheline Syenite 10.00
OM4 Ball Clay 40.00
Silica 10.00

Instructions

Published in "Deep Plates" by Kristin Pavelka, in the Sep/Oct 2011 issue of Pottery Making Illustrated.
Can be applied to leather-hard, bone dry, or bisqued clay.