All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 10.20
Whiting 11.10
Custer Feldspar 73.80
Silica 4.90
Add Amount
Copper Carbonate 0.35
Tin Oxide 1.00

Instructions

Originally published in the October 2010 issue of Ceramics Monthly.