All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 40.00
Nepheline Syenite 10.00
OM 4 Ball Clay 40.00
Silica 10.00
Add Amount
Zircopax 7.00

Instructions

Published in "Confidence in Glazing" by Brian R. Jones, in the January/February 2017 issue of Pottery Making Illustrated.

The piece in the image shown on this page uses Pete's Best Low-Fire Slip with a clear glaze over it.
I typically mix this slip on the thick side because the nepheline syenite and sodium create a slight deflocculation. Wait 24 hours before fine tuning.