All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 1.07
Talc 7.77
Whiting 22.36
Custer Feldspar 30.88
Edgar Plastic Kaolin 12.57
Silica 25.35
Add Amount
Copper Carbonate 6.50

Instructions

Published in "Firing the Hikarigama" by Janet Buskirk, in the Apr 2001 issue of Ceramics Monthly.