All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 55.00
EPK Kaolin 20.00
Silica 25.00

Instructions


Some translucency with somewhat warmer gray color. Limited sheen when fired to cone 9.

This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.