All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
China Clay 20.00
Minspar 200 Feldspar 70.00
Silica 10.00

Instructions


Very white with sufficient translucency. Sample becomes unstable in the cone-9 firing. Glossy sheen.

This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.