All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
China Clay 20.00
Minspar 200 Feldspar 55.00
Silica 25.00

Instructions


Very white with sufficient translucency. Still fairly stable in the cone-9 firing. Pleasantly self glazed.

This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.