All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 40.00
Halloysite Kaolin 20.00
Silica 40.00

Instructions


Very white with sufficient translucency. Sample is fairly stable in the cone-9 firing. Not enough self glazing on the surface.

This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.