All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Cornwall Stone 40.00
Kaolin 15.00
Calcium Carbonate 15.00
Barium Carbonate 10.00
Silica 20.00
Add Amount
Red Iron Oxide 2.50

Instructions


This glaze is not safe for food.

This recipe was sourced from The Ceramic Spectrum: A Simplified Approach to Glaze and Color Development by Robin Hopper.