All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Borax 6.00
OM4 Ball Clay 42.00
EPK Kaolin 42.00
Zircopax 10.00

Instructions

Published in "Carbon Trapping" by Dave Finkelnburg, in the Mar 2013 issue of Ceramics Monthly.