All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 10.00
Talc 6.67
Whiting 7.78
Custer Feldspar 47.78
EPK Kaolin 6.66
Silica 21.11
Add Amount
Red Iron Oxide 11.11

Instructions


This is a very rich warm brown with red hues that run through it. I use this as a liner glaze for most of my pagoda vessels. I like the contrast of dark to light with the flashes of orange, gold, red, and white that the salt/soda firings give me.

This recipe was shared Arlynn Nobel in the May/June 2021 issue of Pottery Making Illustrated.