All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 20.00
Wollastonite 10.00
Nepheline Syenite 30.00
EPK Kaolin 10.00
Silica 30.00
Add Amount
Bentonite 2.00

Instructions

Mid-range clear glaze.

Published in "A House Built for Butter" by Courtney Long, in theMar/Apr 2017 issue of Pottery Making Illustrated.