All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 14.10
Nepheline Syenite 44.40
Ferro Frit 3134 13.10
Kaolin 3.00
Silica 26.20
Add Amount
Tin Oxide 2.60
Copper Carbonate 0.50
Bentonite 1.00

Instructions

Originally published in the October 2010 issue of Ceramics Monthly.