All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gillespie Borate 30.00
F-4 Feldspar 46.00
EPK Kaolin 13.00
Silica 11.00
Add Amount
Manganese Dioxide 10.00

Instructions

Published in "Expanding Your Palette in Mid-Range Firing" by Yoko Sekino-Bové, in the Jan 2011 issue of Ceramics Monthly.