All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 60.00
Spodumene 10.00
Alumina Hydrate 30.00
Add Amount
Bentonite 4.00

Instructions

This recipe was contributed by Elena Renker in the November 2019 issue of Ceramics Monthly.
This is from John Britt's book, Complete Guide to High-Fire Glazes. This glaze is a bit drier but it has a lovely feel to it.