All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Spodumene 15.00
Fusion Frit-38 60.00
EPK Kaolin 25.00

Instructions


This recipe was shared by Rhonda Willers in the March/April 2020 issue of Pottery Making Illustrated.