All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 18.00
Whiting 4.00
Nepheline Syenite 31.00
China Clay 22.00
Silica 21.00

Instructions


This recipe was shared by Mizuyo Yamashita in the June/July/August 2019 issue of Ceramics Monthly.